1.3917, AISI Ni42
Production specification
Square-shape steel standard Download
Plate steel standard Download
Billet standard Download
Flat bar standard Download
wire standard Download
tube standard Download
pipe standard Download
Forging standard Download
casting standard Download
sheet standard Download
round bar standard Download
coil standard Download
Bar stock standard Download
profiled bar standard Download
1.3917, AISI Ni42
Designation by Standards
Brand Name | LH No. | Mat. No. | DIN | EN | AISI |
ALLOY42 | 448 | 1.3917 | Ni42 | - | - |
Chemical Composition (in weight %)
C | Si | Mn | Cr | Mo | Ni | V | W | Others |
max. 0.05 | - | - | - | - | 42.00 | - | - | - |
Description
This alloy is a 42% nickel-iron controlled expansion alloy which has been used in a wide variety of glass-to-metal sealing applications. While the expansion properties of this alloy most closely match 1075 glass, it has also been used in seals fo the 0120 and 0010 glasses. It may also be used with hard glasses if a thin edged tubular seal is used. For seals that are not hydrogen annealed prior to sealing, a variation of this alloy containing small additions fo titanium, Glass Sealing 42 Gas-Free, has been used to promote gas-free sealing characteristics.
Applications
Commonly employed in electronic equipment such as radios, laser systems and thermostats. Alloy has been used for the glass-to-metal seals in electronic tubes, automotive and industrial lamps, transformer and capacitor bushings and other glass-to-metal and ceramic-to-metal applications.
Physical properties (avarage values) at ambient temperature
Modulus of elasticity [103 x N/mm2]: 215
Density [g/cm3]: 8.12
Thermal conductivity [W/m.K]: 74.0
Electric resistivity [Ohm mm2/m]: 0.66
Specific heat capacity[J/g.K]: 0.50
Curie Temperature: 380oC
Coefficient of Linear Thermal Expansion 10-6 oC-1
30-300oC | 30-450oC |
4.0-4.7 | 6.7-7.4 |
Soft Annealing
Heat to 788oC and hold at heat for at least one-half hour per inch of thickness, air cool.
Hardening
This alloy will not respond to hardening by thermal treatment.
Forging
Hot forming temperature: The forging temperature should be 1177-1204oC. Avoid prolonged soaking to prevent sulfur absorption from the furnace atmosphere.
Machinability
The alloy is readily machinable by conventional techniques.
Corrosion Resistance
This alloy has good resistance to corrosion by mild atmospheres, fresh and salt water.
Cold working
The alloy has good ductility and is readily cold worked.
Welding
Any of the conventional welding methods can be used. When filler rod is required, Glass Sealing 42 is suggested.
Related hot word search:1.3917 AISI Ni42 1.3917, AISI Ni42 round bar,1.3917, AISI Ni42 forging,1.3917, AISI Ni42 sheet,1.3917, AISI Ni42 coil,1.3917, AISI Ni42 flat bar,1.3917, AISI Ni42 pipe,1.3917, AISI Ni42 Lrregular
Prev:DIN 1.4773, AISI X8Cr30
Next:1.4000, DIN X6Cr13, AISI 410S